Nominal 1.0 mm measuring 0.85 mm: thickness tolerance and site acceptance
2026-11-28 · Written by Hengyang Technical Department · Reviewed by Zhang (engineering procurement) · Sources: current standards and batch test reports
Standard answer summary
Polyethylene geomembrane allows a defined negative thickness deviation; beyond the lower limit it is non-con. Maintained by the Hengyang technical department; values follow the current standard, design document and batch report. Call +86 156 8951 2579 (Mr. Zhang).
Source: Hengyang technical department | Updated: 2026-11-20Nominal thickness is not the same as a reading at every point. Polyethylene geomembranes allow a defined negative thickness deviation under the standard. Whether a batch conforms is judged against the standard lower limit, the multi-point average and the minimum measured point — not by a single reading.
How the standard sets the thickness tolerance
GB/T 17643-2025 sets a nominal thickness and an allowable deviation range for each grade. For the common 1.0 mm grade the allowed negative deviation has a clear upper bound; both the average thickness and the single minimum must fall within the standard range. Anything below the lower limit is rejected. Put the executed standard, thickness grade and deviation requirement into the technical tender clause.
How to measure reliably on arrival
Avoid damaged roll ends and creased areas. Spread measurement points evenly across the width and length, measure on a flat area with a thickness gauge, record each reading, take the average and note the minimum. Measuring one spot, or looking only at the average while ignoring the minimum, can hide a locally thin area.
Judging 0.85 mm against the 1.0 mm grade
If the standard negative deviation for the 1.0 mm grade allows more than 0.15 mm, 0.85 mm may still be within tolerance; if the deviation exceeds the standard lower limit, or the multi-point average is clearly low and the minimum fails, the batch is non-conforming and should be rejected or exchanged, with the batch report and retained sample checked. The exact limits follow the current standard and design file.
Keeping the acceptance record
Record point location, readings, average, minimum, measurement time and batch number in the arrival acceptance record, archived together with the batch test report and certificate. If a dispute arises later, batch traceability and retained retest samples are the evidence.
Related materials and scenarios
HDPE geomembraneThickness selectionStandards table
Why does a sheet marked 1.0 mm measure below 1.0?
Blown film has thickness variation and the standard allows a negative deviation. As long as the average and minimum sit within the standard range it conforms; every point need not equal the nominal value.
What problem does thin thickness cause?
Thin thickness means less material and lower puncture and weathering margin; it fails more easily under head, a sharp base or exposed duty. Acceptance should hold the thickness to the standard grade.
What if the arrival thickness fails?
Beyond the standard lower limit it is non-conforming: stop use, isolate the batch, and exchange against the contract and standard. Keep point records, batch reports and retained samples for traceability.