What oxidation induction time (OIT) says about a geomembrane formulation
2026-11-28 · Written by Hengyang Technical Department · Reviewed by Zhang (engineering procurement) · Sources: current standards and batch test reports
Standard answer summary
OIT reflects resistance to thermo-oxidative ageing and is a harder indicator of the formulation than any “ho. Maintained by the Hengyang technical department; values follow the current standard, design document and batch report. Call +86 156 8951 2579 (Mr. Zhang).
Source: Hengyang technical department | Updated: 2026-11-20Judging whether a geomembrane will last long-term needs more than thickness and price. Oxidation induction time (OIT) is the time to start oxidation under high temperature and oxygen; a higher value usually means more thermo-oxidative ageing margin, and it is a checkable batch-report index rather than a verbal “guaranteed to last years”.
What OIT measures
OIT is measured by the standard method at a set temperature and oxygen atmosphere, recording the time from start to oxidative exotherm. It reflects the stability of the resin and antioxidant system. A virgin formulation with enough antioxidant usually shows higher OIT; a sheet with regrind or insufficient antioxidant reads clearly lower.
Which indices to read alongside OIT
OIT is not isolated. Read it together with carbon black content (which governs UV weathering), tensile strength and elongation at break, and puncture resistance. Low OIT means thin thermo-oxidative margin; low carbon black means exposed duty ages and cracks easily. Exposed liners, sunlight and freeze-thaw duty place higher demand on both.
How to use OIT in tender and acceptance
Write the executed standard, OIT requirement and carbon black content into the technical clause, and require the batch report to carry the corresponding data. Do not accept only a text promise of “ageing-resistant, lasts years”. High-risk projects can arrange arrival retesting or third-party testing.
Is low OIT unusable?
It depends on the duty. Short-term cover and buried, low-head duty away from light have a lower OIT requirement; long-term exposure, high temperature or chemical duty should choose a sheet with OIT and carbon black at the environmental grade. The index must match the design condition — neither blindly overstated nor lowered at critical parts.
Related materials and scenarios
HDPE geomembraneStandards tableComposite geomembrane
Is higher OIT always better?
Within the conforming range higher OIT means more thermo-oxidative margin, but it still pairs with carbon black, tensile and puncture indices and the duty; one high index does not prove overall performance.
Why is OIT low in regrind sheet?
Regrind has been heat-processed several times; antioxidant is depleted and resin molecular weight drops, so OIT and batch consistency are usually below virgin resin. A low quote often comes with this concession.
How to check the OIT report?
Match batch number, thickness grade, OIT value and the standard requirement; a report cannot be borrowed from another batch. Retest a retained sample on site where needed.
Send us your project conditions
We reply with datasheets, test reports and a quotation within one business day.