Shandong Hengyang New Materials | Geosynthetics plant, Dezhou Geomembrane · Geotextile · Composite liner · GCL Hotline +86 156 8951 2579(Mr. Zhang) 中文EN
INSIGHTS · industry

Welding temperature, speed and pressure: how to set them

2026-11-18 · Written by Hengyang Technical Department · Reviewed by Zhang (engineering procurement) · Sources: current standards and batch test reports

Standard answer summary

Do not copy one number. Trial-weld by membrane grade, thickness and ambient temperature, then lock temperatu. Maintained by the Hengyang technical department; values follow the current standard, design document and batch report. Call +86 156 8951 2579 (Mr. Zhang).

Source: Hengyang technical department | Updated: 2026-11-20

Dual-track hot wedge welding needs both seams molten without burning through. Too hot carbonises the edge; too cold gives a false weld that fails a pressure test.

Speed and temperature move together. Thick sheet needs more heat, usually at lower travel speed. Cold or damp conditions call for preheating and wind protection, not just higher temperature.

Make a trial weld at the start of every shift and record temperature, speed, pressure, ambient temperature and batch. Peel or shear test the coupon before production welding.

Related materials and scenarios

How often should welding parameters be checked?

Every shift, batch change, thickness change, significant temperature change or restart after a long stop.

What if the seam shows a burnt mark?

Cut it out and re-weld. Do not grind it away; check temperature and speed to stop it recurring.

Send us your project conditions

We reply with datasheets, test reports and a quotation within one business day.

Request a quotationEmail us
Call Top